Experiments on anisotropic and rate sensitive strain ratio and modulus of columnar-grained ice

Anisotropic and rate sensitive characteristics of the ratio of lateral strain to axial strain in addition to the rate sensitive effective modulus for columnar-grained freshwater ice and sea ice from the Arctic, have been investigated. Tests were carried out at -20 degrees C, for conditions of no mic...

Full description

Bibliographic Details
Published in:Journal of Offshore Mechanics and Arctic Engineering
Main Author: Sinha, N. K.
Format: Article in Journal/Newspaper
Language:English
Published: ASME 1989
Subjects:
ice
Online Access:https://doi.org/10.1115/1.3257107
https://nrc-publications.canada.ca/eng/view/ft/?id=f8825293-95ad-4356-ba01-c2bcbd21e49c
https://nrc-publications.canada.ca/eng/view/object/?id=f8825293-95ad-4356-ba01-c2bcbd21e49c
https://nrc-publications.canada.ca/fra/voir/objet/?id=f8825293-95ad-4356-ba01-c2bcbd21e49c
Description
Summary:Anisotropic and rate sensitive characteristics of the ratio of lateral strain to axial strain in addition to the rate sensitive effective modulus for columnar-grained freshwater ice and sea ice from the Arctic, have been investigated. Tests were carried out at -20 degrees C, for conditions of no microcracking under uniaxial loads (normal to the length of the grains) in the stress rate range of 1 x 10-3 MN.m-2s- 1 to 1 x 102 MN.m-2 s-1 or an equivalent strain rate range of 1 x 10-7 s-1 to 1 x 10-2 s-1. With increase in stress rate, the ratio increased from about 0.2 to 0.3 in the plane parallel to the columns whereas it decreased from about 0.65 to 0.3 in the plane normal to the columns. A closed-loop controlled test system in association with foil gauges, mounted directly on the specimen, was used. A clipon displacement gauge was used to evaluate the accuracy of the foil gauges. On a étudié les caractéristiques d'anisotropie et de sensibilité au taux du rapport de la déformation latérale à la déformation axiale, ainsi que le module effectif de sensibilité au taux pour de la glace d'eau douce et de la glace de mer à grains prismatiques de l'Arctique. Des essais ont été réalisés à -20 degrees C dans des conditions de non-microfissuration sous des charges uniaxiales (perpendiculaires à la longueur des grains) dans la plage de taux de contrainte de 1 x 10-3 MN.m-2s-1 à 1 x 102 MN.m-2s- 1, soit une variation équivalente du taux de déformation de 1 x 10-7s-1 à 1 x 10-2s-1. Dans le cas d'augmentation du taux de contrainte, le rapport est passé d'environ 0,2 à 0,3 dans le plan parallèle aux prismes, tandis qu'il est passé d'environ 0,65 à 0,3 dans le plan normal. On a utilisé un appareil d'essai fonctionnant en boucle fermée associé à des jauges à feuille mince montées directement sur l'éprouvette. Pour évaluer la justesse des jauges à feuille mince, on s'est servi d'une jauge de déplacement clipsable. Peer reviewed: Yes NRC publication: Yes